  1. Default 250ex problems

    So finally got a chance yesterday to fire up the machine and start a little job. Well I didn't get far at all. I fire the machine up and the display basically reads 888, it will fluctuate up and down a few numbers. But changing settings does nothing. It won't strike an arch or really do anything. Has anyone seen this problem? It's brand new, unfortunately I've had it just over 30 days. Tech gave me a rma. That's all they had to say. Very bummed as I was excited to use it and this now delays a project I wanted to start/finish.

  2. #2

    Default

    You can remove the rear cover and the metal cover, and check your connections. Unplug them and reseat them. It won't hurt anything, providing you unplug your unit first for 15 minutes before starting work.

    Exactly when did you purchase it?

  3. Default

    Quote Originally Posted by performance View Post
    You can remove the rear cover and the metal cover, and check your connections. Unplug them and reseat them. It won't hurt anything, providing you unplug your unit first for 15 minutes before starting work.

    Exactly when did you purchase it?
    April 23. What connections?

  4. #4

    Default

    Any and all, particularly leading from the display board.

  5. Default

    Same thing happened to my brand new 250 ex. I had it for about two weeks and display started displaying showing random numbers and the welder ceased to function. I ended up getting rid of the welder and moved on to another brand.

    Hope Everlast service can help you.

  6. #6

    Default

    FWIW: The display will show random numbers in pulse mode.

  7. #7

    Default

    Quote Originally Posted by performance View Post
    FWIW: The display will show random numbers in pulse mode.
    set amperage pulse off then select hi/lo pulse. to adjust turn pulse off, set ,then pulse on
    RTFM

  8. #8

    Default

    Quote Originally Posted by Coventry View Post
    Same thing happened to my brand new 250 ex. I had it for about two weeks and display started displaying showing random numbers and the welder ceased to function. I ended up getting rid of the welder and moved on to another brand.

    Hope Everlast service can help you.
    what brand did you go with and what did you do with ur everlast machine?
    250 ex
    205 mig
    milwaukee grinder
    140e mig

Similar Threads

  1. A PowerTIG 250EX and problems
    By L98fiero in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 08-22-2015, 08:43 PM
  2. 250ex arc problems welding on ac but not dc ?????
    By slufoot2005 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 11
    Last Post: 10-12-2013, 02:48 PM
  3. 250EX problems with foot pedal
    By Boosted P in forum TIG Welding (GTAW/GTAW-P)
    Replies: 20
    Last Post: 03-09-2012, 03:51 AM
  4. New 250EX owner, a few problems
    By Adambomb in forum TIG Welding (GTAW/GTAW-P)
    Replies: 109
    Last Post: 03-18-2011, 03:11 AM
  5. shipping problems with new 250ex?
    By Bulldad3 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 02-28-2010, 02:37 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •