How to minimize spatter?
My setup includes a Powermig 250 with a #4 bottle of argon/co2 mix flowing ~10 cfm. My wire feed rates seems to average roughly 10x my voltage. The beads look good and after cutting a few apart I'm getting good penetration on the welds. My last setup was 3/16" plate to 3/16" plate in a T joint setup. Voltage was 17.9, wire feed was 175-180. My problem is there is just a ton of spatter. While writing this post, I was browsing around and saw a lot of recommendations for up to 25 CFM on the shielding gas. I have set it that high before, and it seems like an awful lot of gas flow, and even then there was a lot of spatter. What would you guys recommend?
Poewr I-Mig 205P
Powertig 185