Using a power tig 185. Most online guided for invertwe machines suggest yellow, red or blue tungsten. I have tried all of them and can't get any to work. If I use 3/32 green tungsten, 50-50 EN/EP balance, 15ish cfm, #8 cup, I can get a bead to form and lay down meh puddles. Frequency does what it's supposed to with higher narrowing the arc and lower widening it.

I have tried gold, orange, red and black 3/32 tungsten and all have the same result. The aluminum pits, turns black, and melts away in an overheated mess before a clear puddle forms. I have tried turning the balance to 80% EN which does nothing, to 80% EP which just balls up the tungsten and makes it run away from the part. I have tried the lowest frequency setting up to the highest. It's a relatively new bottle of argon, so I guess it could be bad gas, but like stated, I can get a nice workable puddle with green tungsten using this tank of gas. I have tried no cleaning, wire brush cleaning, and wire brush plus acetone cleaning. Results don't change at all.

So I guess my question boils down to, how the hell do you guys get yellow or red tungsten to weld aluminum? I just can't figure out the settings.