Originally Posted by
AnimalMother
so your saying. regardless of where i have the amps set on the panel i can crank the pedal down and get full 200 out of it? i can't set a limit of amps on the panel when running the pedal?
Your pedal should have an amps limit knob on the side if it is that style. But you don't use the display, instead you have to use the printed scale on the pedal knob.
Long arc, short arc, heliarc and in-the-dark!