    Ok I wanted to get a few different mig wires to see what works best on galvanized so I got blue demon er70s-2, blue demon silicon bronze, blow demon e71t-gs, Lincoln er70s-3, and er70s-6. Just wondering how you guys like blue demon? I read good reviews in it that's why I purchased plus little easier to get on eBay than Lincoln stuff.

  2. #2

    Default

    Any wire works fine when you grind the zinc off the weld area and spray it with cold galvanizing after you weld. I'm sure you know to not breath the smoke from galvanizing.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3
    Join Date
    Mar 2016
    Location
    Okinawa, Japan
    Posts
    30

    Default

    Yeah I usually have a big fan blowing it out since it's flux core I can have good airflow. I was using Lincoln ER70S-6 with 80/20 Argon/CO2 and holy #### the spatter I was getting. I know it's mostly the galvanizing causing the spatter but I'm going to try some different wires anyways. Plus holy #### does this Lincoln wire grind hard, it's taking me longer to grind all the seams out smooth than it is to do the whole project. Hoping the silicon bronze wire works out, I heard it grinds real nice. It's just a powder coating oven so really just filling in the seams for the sheet metal.

  4. #4

    Default

    Quote Originally Posted by pavetim View Post
    Yeah I usually have a big fan blowing it out since it's flux core I can have good airflow. I was using Lincoln ER70S-6 with 80/20 Argon/CO2 and holy #### the spatter I was getting. I know it's mostly the galvanizing causing the spatter but I'm going to try some different wires anyways. Plus holy #### does this Lincoln wire grind hard, it's taking me longer to grind all the seams out smooth than it is to do the whole project. Hoping the silicon bronze wire works out, I heard it grinds real nice. It's just a powder coating oven so really just filling in the seams for the sheet metal.
    Try holding a tighter arc (shorter stickout). With flux core you can take the nozzle off to see better. Did you switch polarity for flux core ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. #5
    Join Date
    Mar 2016
    Location
    Okinawa, Japan
    Posts
    30

    Default

    Yes I switched the polarity

Similar Threads

  1. Replies: 6
    Last Post: 10-11-2014, 06:09 PM
  2. Helmet Shootout: W60 Truesight vs Harbor Freight Blue Flame vs HSL-100 fixed shade
    By jakeru in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 43
    Last Post: 11-19-2012, 08:42 PM
  3. Red/Blue Quick-Release Water Line Connectors
    By X83 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 10-04-2012, 11:16 PM
  4. why buy green instead of red or blue?
    By backhoe in forum Introduce Yourself
    Replies: 29
    Last Post: 01-19-2012, 04:30 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •