  1. #1
    Join Date
    Aug 2014
    Location
    Westerville, Ohio
    Posts
    72

    Default Robust garage floor concrete patch with welded rebar.

    The garage slab is to the right, top, and left of the photo. Six inch deep half inch diameter holes were drilled into the garage slab. Rebar was then pounded into the holes. Additional rebar was then welded to the pieces sticking out of the holes tying the individual spans together.

    No rebar ties the driveway slab and the garage slabs together. They suffer different temperature, weather, and load characteristics. The expansion joint between the two will remain just that, an expansion joint.

    Pure utility, nothing glamours or creative. It is, however, exceedingly stout concrete repair.


    Click image for larger version. 

Name:	100_4049.jpg 
Views:	611 
Size:	147.3 KB 
ID:	13492

  2. #2
    Join Date
    Aug 2014
    Location
    Westerville, Ohio
    Posts
    72

    Default

    Photo of finished and cured concrete patch. The gloves are for scale. Sorry about the shadows, the low angle of the sun through the trees makes for the distracting contrasts.


    Click image for larger version. 

Name:	100_4118.jpg 
Views:	467 
Size:	142.9 KB 
ID:	13496

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,662

    Default

    Long arc, short arc, heliarc and in-the-dark!

  4. #4
    Join Date
    Aug 2014
    Location
    Westerville, Ohio
    Posts
    72

    Default

    Geico gecko gloves?

  5. #5

    Default

    Looks like it will do the job. Sometime simple it all you need.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Concrete Plug and Fence Post Pulling Lever
    By fyidiy in forum Other Custom Fabrications
    Replies: 2
    Last Post: 04-29-2017, 10:11 PM
  2. Tigging a radio patch panel?
    By Dne007 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 19
    Last Post: 02-07-2014, 12:20 AM
  3. Pressure washer trailer patch
    By chadford in forum Welding Repairs
    Replies: 0
    Last Post: 11-28-2013, 02:27 PM
  4. Concrete planter
    By CGCINC in forum Personal Projects (no welder required)
    Replies: 12
    Last Post: 05-30-2013, 02:07 PM
  5. project 4 from ogorir: inner quarter panel patch
    By ogorir in forum On Road Fabrication
    Replies: 1
    Last Post: 10-25-2011, 04:23 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •