  1. Question Wire Speed Values

    I have a new POWER I-MIG 140E. I am new to welding.

    I ran it through every wire speed block (10) on the dial. I ran each block 3 times at 6 seconds and averaged the speeds,

    60-80-110-120-140-180-220-240-270-310. I realize that it's not exact science.

    The manual states a max speed of 350.

    Any concerns here?

    Thanks
    Gordon

  2. #2

    Default

    Quote Originally Posted by thegoschman View Post
    I have a new POWER I-MIG 140E. I am new to welding.

    I ran it through every wire speed block (10) on the dial. I ran each block 3 times at 6 seconds and averaged the speeds,

    60-80-110-120-140-180-220-240-270-310. I realize that it's not exact science.

    The manual states a max speed of 350.

    Any concerns here?

    Thanks
    Gordon
    It's my understanding that the wire speed increases when you start an arc on all of the Everlast mig machines.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

Similar Threads

  1. wire speed accuracy?
    By mts211si in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 20
    Last Post: 11-17-2015, 08:19 PM
  2. iMIG 140e Wire Speed
    By Slartybartfa in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 0
    Last Post: 01-16-2015, 01:58 AM
  3. I-Mig 205 wire speed not high enough?
    By camboscams in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 4
    Last Post: 01-21-2014, 03:41 PM
  4. I-MIG 250p Low Wire Speed
    By zoama in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 8
    Last Post: 03-05-2012, 01:49 AM
  5. Replies: 26
    Last Post: 02-22-2012, 12:25 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •