  1. Default Power tig 250ex issue

    Hey fellas,
    Just need a little info. My welder is now very finicky about the length of the tungsten. Short stick out no puddle just some little melting. Normal stick out runs fine. Lengthen it some it just digs into the metal, no puddle. I use to be able to vary the length depending on the work piece but now it's very finicky. Does it with the pedal and torch switch operation. I have no clue. All torch pieces have been changed out already. Thx!
    Everlast PowerTig 250EX w/ PowerCool W300
    Everlast PowerMig 275S
    Everlast PowerPlasma 60S

  2. Default

    Gee,

    Since it "runs fine" with a "normal stick out", it may just be a setting, like too high a flow of gas for the cup size that you're using. Or, if that's not it, I'd rule out the gas itself, by just swapping out a bottle. And if you're not using one already, put a gas lens on the torch.

    Maybe some pictures of what "normal", etc., looks like would help.


    Quote Originally Posted by Blaze View Post
    Hey fellas,
    Just need a little info. My welder is now very finicky about the length of the tungsten. Short stick out no puddle just some little melting. Normal stick out runs fine. Lengthen it some it just digs into the metal, no puddle. I use to be able to vary the length depending on the work piece but now it's very finicky. Does it with the pedal and torch switch operation. I have no clue. All torch pieces have been changed out already. Thx!
    Everlast 210 EXT (2015)

    www.youtube.com/newjerusalemtimes

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,662

    Default

    Quote Originally Posted by Blaze View Post
    Hey fellas,
    Just need a little info. My welder is now very finicky about the length of the tungsten. Short stick out no puddle just some little melting. Normal stick out runs fine. Lengthen it some it just digs into the metal, no puddle. I use to be able to vary the length depending on the work piece but now it's very finicky. Does it with the pedal and torch switch operation. I have no clue. All torch pieces have been changed out already. Thx!
    Settings and material please. Sounds like something to do with gas to me, too. Can't think of anything in a power supply that would even care about stickout. Are you using a gas lens? The tungsten to workpiece distance matters, and needs to be right, but stickout can vary a lot with the right torch parts and gas settings with no problems.
    Long arc, short arc, heliarc and in-the-dark!

  4. Default

    Nevermind. Tried to do an aluminum project yesterday and it would only give me the hf start arc. Intermittent issue so something must be about to go. Going to contact tech support.
    Everlast PowerTig 250EX w/ PowerCool W300
    Everlast PowerMig 275S
    Everlast PowerPlasma 60S

Similar Threads

  1. Issue with Power TIG 250EX
    By karter59 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 09-20-2016, 01:12 PM
  2. 250EX issue
    By Blaze in forum TIG Welding (GTAW/GTAW-P)
    Replies: 21
    Last Post: 07-29-2016, 01:12 AM
  3. PowerTig 250Ex weird issue.
    By dmost in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 02-22-2014, 12:39 PM
  4. Power Ultra 205 issue
    By turpehar in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)