So I am confused what is the duty cycle on this unit. on page says 60% at 60amps and another say 100% at 63 amps. Which is correct?
Also while i am at it. I am putting this on a plasma table replacing a ever-last unit that well =) shouldn't be used for cnc lol, and was looking at using using the pt-60 machine head rather then the pt-80. I don'tplan on cutting over 1/4 or maybe 3/8 at most would the pt-60 torch be able to handle that? I do a lot more sign work where the lower amp/finer tips would be more beneficial, but still want to be able to cut 1/4. Would rather not have to run two heads or be switching heads.
Thanks




plan on cutting over 1/4 or maybe 3/8 at most would the pt-60 torch be able to handle that? I do a lot more sign work where the lower amp/finer tips would be more beneficial, but still want to be able to cut 1/4. Would rather not have to run two heads or be switching heads.