Originally Posted by
2horses
Well, I got to try my torch today. I must have overheated it because it's leaking. Can i just replace the torch or do i have to buy all new hoses?
Usually it's not the torch, but the power line that fails first. If you're lucky you can just replace that. However, if it got real hot, it might have melted holes in the other two lines. All the parts are available separately, so you can replace what you need.
BTW: CK makes a fuse block connector that will save your torch and lines if you lose water flow for any reason.
Last edited by Rambozo; 03-08-2017 at 11:50 PM.