  1. Default Smoother weld on AC aluminium with the torch positive, not negative.

    I thought that the 200dx when welding aluminium in AC was meant to have the torch negative?


    After switching my torch to positive, then rotating the balance clockwise to maximum the machine seems smoother now.


    Is that the way it is meant to be run then? torch +ve for AC aluminium ?

  2. #2

    Default

    Rtfm!**&&*%

Similar Threads

  1. Just want to hand out some positive Kudos;
    By Baronsbest in forum Pre-sales, Sales and Shipping questions
    Replies: 2
    Last Post: 01-31-2019, 01:29 AM
  2. bad contamination. cannot weld aluminium
    By js quebec in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 09-23-2017, 07:51 PM
  3. Negative threads delegated?
    By FabGTO in forum Customer Testimonials
    Replies: 8
    Last Post: 04-12-2011, 05:53 AM
  4. Another aluminium welding cart
    By AussieChris in forum Other Custom Fabrications
    Replies: 3
    Last Post: 02-07-2011, 12:32 PM
  5. Where are the negative reviews?
    By generatorlabs in forum Customer Testimonials
    Replies: 38
    Last Post: 07-21-2010, 02:35 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •