I've had a POWER IMIG 250P for several years and have fumbled through a couple of spools of wire but proper settings have me confused. In trying to figure out what I should be starting with checked several different manufacturers charts and as an example, for 0.035 ER70S-6, 75:25 mix on 1/4" steel the recommended settings from three different manufacturers are 19/320, 20/250 and 23/305. Given that, are there rules of thumb one can use? I do understand that getting better requires experience but having a reasonable place to start seems like a good idea.
On a side note, is there a way to retrofit the welder for a spoolgun? Everlast says no but there are some pretty inventive people on the forum.




 
					
					 
							