Share
Results 1 to 9 of 9

Thread: PM 256 Hi-Freq quit working

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Unhappy PM 256 Hi-Freq quit working

    I had big plans this weekend to get caught up on projects, but no joy. I went to use the plasma cutter and the high frequency pilot arc did not work, I tried the TIG - no high frequency there either. I can start the both the plasma and TIG by scratching.

    Its been about 3 weeks since I last used the machine and its unplugged when not in use. Machine was purchased new in April, is there anything I can do to fix it?

    Thanks,

    Tony

  2. #2

    Default

    Tony,
    You can call Mike and he should be able to walk you through diagosing it, and more than likely get you up and running.

  3. #3

    Default

    Quote Originally Posted by performance View Post
    Tony,
    You can call Mike and he should be able to walk you through diagosing it, and more than likely get you up and running.
    Thanks Mark, what number can I reach him at? I tried 650 588 8082 x203 and it went to voice mail - obviously on the weekend.

    Tony
    Last edited by Tony_F; 07-03-2010 at 08:55 PM.

  4. #4

    Default

    I was able to get in touch with Mike, we adjusted the hi freq points at the front of the unit, they spark when the troch trigger is activated, but still no pilot arc or HF at the torch.

  5. #5

    Default

    Machine is on its way back to Everlast for an exchange. We'll see how long that takes, as they may be out of stock until later in the month.

  6. #6

    Default

    Tony,

    That shouldn't be a problem...By the time the machine is received, they should be able to ship it right out with no delay.

  7. #7

    Default Replacement Here!

    I rec'd the replacement welder today, the box was in the usual condition, had a few tears on the side, but not totally squashed. The machine seemed fine. Anyway, the only function I had time to try was the plasma as I'm in need of it - it seemed to work OK - hi-freq is back! I'll post a few pictures of the project this weekend.

    Thanks Mike and everyone for the support and getting it replaced.

    Tony

  8. #8
    Join Date
    Jul 2010
    Location
    In the Land of CoRn
    Posts
    69

    Default

    Quote Originally Posted by Tony_F View Post
    I rec'd the replacement welder today, the box was in the usual condition, had a few tears on the side, but not totally squashed. The machine seemed fine. Anyway, the only function I had time to try was the plasma as I'm in need of it - it seemed to work OK - hi-freq is back! I'll post a few pictures of the project this weekend.

    Thanks Mike and everyone for the support and getting it replaced.

    Tony
    Good to hear! I like your initial review write up! I was curious what type of ball valves did you use for switching between air and argon?

    I went to the local lowes, and they suggested using ones for natural gas, but the handles were too small.

  9. #9

    Default

    Quote Originally Posted by Slick View Post
    Good to hear! I like your initial review write up! I was curious what type of ball valves did you use for switching between air and argon?

    I went to the local lowes, and they suggested using ones for natural gas, but the handles were too small.
    Sorry Slick I just saw your question..

    http://www.mcmaster.com/

    - 4112T23 COMPACT HIGH-PRESSURE BRASS BALL VALVE, 1/4" NPT FEMALE X MALE, LEVER HANDLE
    - 50785K72 MED-PRESSURE BRASS THRD PIPE FITTING, 1/4" PIPE SIZE, TEE
    - 5346K16 BRASS BARBED HOSE FITTING, ADAPTER FOR 5/16" HOSE ID X 1/4" NPTF PIPE
    - 50785K43 MED-PRESSURE BRASS THRD PIPE FITTING, 1/4" PIPE SIZE, MALE X FEMALE 90 DEG ELBOW
    - 50785K12 MED-PRESSURE BRASS THRD PIPE FITTING, 1/4" PIPE SIZE, NIPPLE, 1-1/2" LENGTH

Similar Threads

  1. 325 Arc starting issues, spudders on hi freq.
    By gorillam in forum TIG Welding (GTAW/GTAW-P)
    Replies: 16
    Last Post: 02-05-2017, 06:21 PM
  2. 185 solenoid quit working..??????
    By stretch in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 06-30-2016, 06:49 AM
  3. HF starts quit working - PowerTIG 200DX
    By Timebandit in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 09-04-2014, 03:04 PM
  4. PP256 High-Freq. wont turn off!!!
    By tensecond408 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 03-07-2014, 10:12 PM
  5. Replies: 6
    Last Post: 10-12-2012, 03:25 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •