Share
Results 1 to 9 of 9

Thread: Would like assistance with setting parameters on my 2017 Power i TIG 201

  1. Default Would like assistance with setting parameters on my 2017 Power i TIG 201

    If ignorance is bliss, that makes me a very happy man. Just got my i TIG 201 last month. I've been welding for about 2 years on a mig machine. Decided to try TIG and liked the specs on this machine. That being said, I'm a 75 year old retired GI that is having difficulty getting all the knobs, dials and whistles working together on this machine. (My MIG welder pretty much automatically sets up & doesn't require much brain power.) I want to TIG light weight metal. Basically 18 gauge to 14 gauge steel. I've read the manual numerous times but cannot seem to get things straight. Sure would appreciate somebody giving me a simple starting point. After I retired from military I taught special needs students for 17 years......therefore I'd really like somebody to do the same for me. I mean, turn torch trigger knobs to X & Y. Seconds knobs to X & Y. Pulse knobs, etc. I've been either too hot, too cold, etc. so far in practice and I sure could use some assistance. Thanks. Fred

  2. Default

    Sure,

    I'll link to a quickie video on the unit below.

    And I'll recommend that you don't use the pulse function to begin with. Also, it may be better for you not to use a foot pedal, to begin with, as DC TIG welding doesn't really need it. That will allow you to focus more on torch and filler control, at first. Just adjust the amps at the panel like you would on Stick or MIG until it's about right, then you can compensate for heat inputs with travel speed and filler amount. After you get comfortable with the two-handed portion of TIG, then introduce the foot pedal. I mean, on my DC-only TIG unit, it was foot-pedal capable, but as an option, which I never bought, and that was never a problem to me. Of course, when I got an Everlast AC/DC unit for doing aluminum TIG, a remote amperage device became a near absolute necessity.

    https://www.youtube.com/watch?v=spy5FbbiXCQ
    Last edited by christian; 03-02-2018 at 07:09 PM.
    Everlast 210 EXT (2015)

    www.youtube.com/newjerusalemtimes

  3. Default

    Thanks for the reply. I've probably watched Chuck go thru the 201 YouTube about 20 times. He knows what he is talking about but it doesn't address the nitty gritty that I'm in need of. I really and truly need a "cheat sheet" to get me started in the right direction.
    Last edited by Dr Fred; 03-02-2018 at 08:14 PM. Reason: spelling correction

  4. Default

    Well,

    Try a bead on plate with no filler, just get a puddle started and move.

    I'd start with 1/8" plate/sheet first. Use a 3/32" tungsten for that.

    When you graduate to the thinner stuff a 1/16" tungsten may be the better choice. But don't take a 1/16" tungsten over 100 amps for very long.

    Weld.com has a lot of TIG videos.

    https://www.youtube.com/watch?v=0ctmbCiHD6Y&t=23s
    Last edited by christian; 03-02-2018 at 08:35 PM.
    Everlast 210 EXT (2015)

    www.youtube.com/newjerusalemtimes

  5. #5

    Default

    Compared with Mig, Tig has an uphill learning curve. This first thing I learned is how to sharpen up Tungsten because I dipped it so often. Stick to the basics, just like anything worth while, it requires time and effort. Many of us thank you for your service.
    Everlast 250EX with cooler and WP20 Torch
    Millermatic Mig Welder
    Gas welding setup
    A bunch of Snap-On tools
    And a Brain

  6. #6

    Default

    Here's my favorite teacher... and thanks for your service to our country.

    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  7. Default

    Thanks... Can use all the help I can get.

  8. #8

    Default

    Watching Jody is like watching pro golf, he makes it look easy! Yet he has volumes of excellent information and videos.
    Everlast 250EX with cooler and WP20 Torch
    Millermatic Mig Welder
    Gas welding setup
    A bunch of Snap-On tools
    And a Brain

  9. Default

    Thanks for the support!!!

Similar Threads

  1. 2017 model year
    By runon in forum General Welder Questions
    Replies: 6
    Last Post: 07-28-2016, 04:49 AM
  2. Erractic arc at low AC setting
    By Sage Hill in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 9
    Last Post: 02-14-2016, 10:59 PM
  3. Setting up my air compressor for the Power Plasma 50....?
    By CGCINC in forum Everlast Plasma Cutters (PAC)
    Replies: 13
    Last Post: 07-06-2012, 06:14 PM
  4. AC / DC Setting is backwards?
    By JonS in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 05-02-2012, 02:25 AM
  5. Welding calculator parameters
    By rengaw21001 in forum Forum related Questions
    Replies: 5
    Last Post: 10-21-2010, 04:17 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •