  1. Default Water cooled 200DX aluminum issues since new

    Ok, I bought my 200dx setup about 2.5 years ago. For the longest time I did not have 220 in my garage so I ran the welder on 110. I was do9ng a lot of thin stainless and some thin aluminum tubing. Welds great onstainless, but the aluminum, it always has struggled to keep the arc going until i dab filler rod. Once fuller is applied, the arc is nice and smooth. Before filler is added, i can hear he machine making the noise it makes if you were told hold the torch in the air and hit the pedal.. the buzzing noise. It's like until filler is applied, it is not getting a good solid arc. I thought it was because I was running it on 110. I recently got 220 service in my garage and it is the same outcome. I weld a ton of aluminum at work, but with a precision tig275. My inverter is a lot different at home. Anything I can do to fix this? Also, why does it happen, and is it normal? Thanks

  2. #2

    Default

    Torch in negative? Balance settings? Tungsten type/size? Let us know and maybe we can help out here.

  3. Default

    Torch is in negative. It welds stainless beautifully, done alot of welding with it. Right now the settings are 50% balance, 90 frequency, red throated 3/32 tungsten

  4. #4

    Default

    Quote Originally Posted by Bad1gdsm View Post
    Torch is in negative. It welds stainless beautifully, done alot of welding with it. Right now the settings are 50% balance, 90 frequency, red thoriated 3/32 tungsten
    I think your balance should be between 25 and 35. I prefer 2% lanthanated tungsten. Check your work clamp connection and try clamping directly to your work piece.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. #5

    Default

    50% will make for harder starts. Set the unit at the minimum (30%).

  6. #6

    Default

    Don't try to ball the tungsten on an inverter machine. You can keep it pointed for more control.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

Similar Threads

  1. Water cooled torch getting hot?
    By 2horses in forum TIG Welding (GTAW/GTAW-P)
    Replies: 10
    Last Post: 04-01-2017, 07:29 AM
  2. Using water cooled torch as air cooled?
    By Fusion in forum TIG Welding (GTAW/GTAW-P)
    Replies: 16
    Last Post: 01-16-2014, 11:08 AM
  3. water cooled torch
    By D.C. Metal Designs in forum General Welder Questions
    Replies: 7
    Last Post: 08-11-2010, 05:01 AM
  4. Water cooled torch question
    By madcratebuilder in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 07-19-2010, 02:08 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •