255 EXT Help, something went wrong with pulse
Been doing a bunch of pulse welding with my brand new 255EXT on round aluminum tube to dial in the best settings. Everything was going great laying down some excellent beads. All of sudden it changed sound and seem like it wasn't giving me the same amps. Welding at 205 amps, took my helmet off and floored it and it will only give me about 75 to 100 amps on the hot side (welding amps) of the pulse??? Shut of the pulse and floored it and goes right up to the 205 amps I have it set at. Any thoughts? All of my work is on a positioner with stationary torch holder for consistency so everything is the same every time.
1/8" 2% Lanthenated tungsten sharpened to a point
12 to 15 CFH
3/32 4043 filler rod
Last edited by travis1693; 09-20-2018 at 12:36 AM.