Supercut 50P Overcurrent light
have not been on here for a while, Decided to use the 50P today to cut the end off a 48" round tank 3/8" material. stopped several times during the cut and the last time no spark trap was clean as i have a dryer. Let it set for at least an hour as i finished up with the torch still nothing any ideas or is it trash.