    Hi there, yes I'm a rookie! I bought a MST 251Si back in 2016 and have very limited use with it (maybe 3 hours). I'm a retired hobbyist and I'd like to learn more about setup of the welder. My other machines had a chart on the cover that would start you in a direction to go and you make adjustments on the fly. I'd like to know what other machines that have a voltage and ipm wire speed chart on their machines are comparable to the MTS 251Si. I'm not a professional welder but would like to know more on where to start instead of listen and adjust to the bacon frying sound. I looked at red & white machines that were close to the 251Si and the voltages and wire speeds were different. If there is a machine with a chart thats close to what I need to start the setup I'd be greatful on knowing which on. Thank you in advance.

  2. #2

    Default

    I recommend using the synergic feature. Use about 1 amp per thousandth of an inch. Easiest way.

  3. #3
    Join Date
    Jul 2016
    Location
    San Diego, CA & Minneapolis, MN
    Posts
    12

    Default

    Thank you, I'll give it a try.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •