  1. Default PowerARC 161STH pulse and other features

    I think it was this machine that somebody from Everlast posted some specs that are not in the manual.

    If I remember correctly (and I may not) there is a preset pre-flow of 0.5 sec, there is a preset upslope of 8 sec starting at 5 amps, the downslope ending amperage is preset at 5 amps (?) and I know the pulse background percentage and time are preset, but I don't know what settings they are.

    Are any of these numbers correct?

    Does pulse only work in 4T or maybe 2T, but not with a foot pedal?

    Do the upslope and downslope only work in 4T or maybe 2T, but not with a foot pedal?

    Having the presets saves from having to set everything and from having to know where to set everything.

    Do these features function?

    The manual doesn't seem to say much.

    If some or all of these features onlt work in 4T then they wouldn't work with a foot pedal.

    They might be good features in 2T, but I thought I saw posted somewhere that they work in 4T mode only.

    I have a Power i-TIG 200T and has a lot of manual settings, but what really sticks out with it is the 26 TIG torch and cable are heavy to work with.

    The 17 TIG torch and cable with PowerARC 161STH would seem handier and the cable is the same that can be used with a number 9 TIG torch.

    Buying a foot pedal for the 161STH would cost as much as buying a smaller TIG torch and cable for the 200T though.

    I can understand not using low speed pulse with a foot pedal, but there are some techniques that use high peed pulse with a foot pedal for stainless steel and some chrome moly.

    It seems that the 161STH could save from having to set the pre-flow, the upslope time and starting amperage, the pulse background amperage and pulse time.

    I know downslope time is adjustable, but I think downslope amperage is fixed and preset to the minimum.

    It looks like a easy setup with some good features, but the manual doesn't cover the details much.

  2. #2

    Default

    No,
    You don't remember right. Pretty far off on most of them. Upslope is fixed, but not at 8 seconds. Just a second or less IIRC.

    Here is the link to the unit.
    https://www.everlastgenerators.com/p...owerarc-161sth

    I think you have some units mixed up. The Purpose of the PowerARC 161STH is to offer an equally capable Stick welder as well as a decent DC TIG welder. Slope doesn't work with the foot pedal setting. Pre/Post Flow do.

  3. Default

    Quote Originally Posted by performance View Post
    No,
    You don't remember right. Pretty far off on most of them. Upslope is fixed, but not at 8 seconds. Just a second or less IIRC.

    Here is the link to the unit.
    https://www.everlastgenerators.com/p...owerarc-161sth

    I think you have some units mixed up. The Purpose of the PowerARC 161STH is to offer an equally capable Stick welder as well as a decent DC TIG welder. Slope doesn't work with the foot pedal setting. Pre/Post Flow do.
    Thank you. That's why I asked, because I didn't remember the details and they may have been from an older unit. I just noticed that some of the details seemed to be missing, but I'll see if i can read more closely about it.

    I take it the pulse doesn't work with a pedal?'

    Does slope only work in 4T not 2T?

    Pulse only in 4T not 2T?

  4. #4

    Default

    Quote Originally Posted by BikeShop View Post
    Thank you. That's why I asked, because I didn't remember the details and they may have been from an older unit. I just noticed that some of the details seemed to be missing, but I'll see if i can read more closely about it.

    I take it the pulse doesn't work with a pedal?'

    Does slope only work in 4T not 2T?

    Pulse only in 4T not 2T?
    Slope works with the torch switch. 2 or 4t

    Pulse works with all modes. There's no reason it shouldn't

  5. Default

    Quote Originally Posted by performance View Post
    Slope works with the torch switch. 2 or 4t

    Pulse works with all modes. There's no reason it shouldn't
    Thank you.

    I had seen some specs for some simplified machines and some functions would only work in 4T mode.

    I didn't see it mentioned in the manual if a certain mode had to be used for certain features to function.