I searched the forum but didn't find an answer.
On a multi-process welder, what's the best way to manage multiple types of gas? For example, a MIG and TIG machine like the 251Si. I'd usually want 80/20 for MIG and 100% Argon for TIG. However, I certainly don't want to change tanks every time I switch process. That would get old really fast. Perhaps I could use a Wye fitting, connect the two tanks, then purge the line when switching process. Or, is there a better way?