Figured I'd post here since my question is stick specific even though I've got a multi-process PU205.
I see the special 6010 port advertised on the power arc 160 and 200. What exactly does that do? Does the fact that my PU205 doesn't have that port mean that I shouldn't be using 6010? Just curious since I just bought some 1/8" 6010 for my PU205 for a friend to stick weld some boxing plates on a truck frame (53 F-100) for me and it seems to sputter randomly and lose the arc. My buddy's a pretty proficient welder especially with stick and on his AC tombstone welder he was getting perfect welds on my truck frame but with the frame back at my house using 6010 on my PU205 he can't pull a consistent bead to save his life, it drops every couple inches. It's definitely not a ground problem (upgraded to the pro Tweco ground clamp on my PU205) or a operator skill problem.
Just curious if the lack of the special 6010 port means I should be using 6011 or some other rod?
Thanks in advance for any feedback on this.
Ralph




Reply With Quote