    Here's a really cool trick I discovered while overthinking a solution for tungsten grinding.

    It's just a small block of 1/2 Al with a 7/64 hole drilled in it and a pin vise. The grinder is a Home Depot 50.00 special.



    I did 10 2% lanth's in 5 minutes. The block is not mounted so you just hold it with one hand and spin the pin vise with the other.
    Steve

    Miller 212
    Everlast 250EX
    Everlast PowerPlasma 60
    Victor O/A
    Current Project: 21' Jet Sled Rat Boat.

  2. #2

    Default

    also try a cordless drill

  3. #3

    Default

    Quote Originally Posted by jeffmel1 View Post
    also try a cordless drill
    I've done that and believe it or not, this is tons faster and eaiser to control.. Weird that such a simple device can make life so much easier. I made a litte better one last night and drilled holes in it for all the sizes of electrodes that i use. I'm gonna carry it in my pocket. It works on any grinder.
    Steve

    Miller 212
    Everlast 250EX
    Everlast PowerPlasma 60
    Victor O/A
    Current Project: 21' Jet Sled Rat Boat.

Similar Threads

  1. Sharpening Tungstens
    By DaveK in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 06-02-2015, 04:50 AM
  2. This would be cool
    By dzljon in forum Metal Art
    Replies: 1
    Last Post: 01-05-2015, 10:52 PM
  3. What is your prefered method to cleaining metal before tig welding
    By turbo_bully in forum General Welding Questions
    Replies: 5
    Last Post: 08-24-2011, 12:20 AM
  4. "Lay Wire Method"
    By www in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 08-19-2010, 03:23 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •