					On my 250EX I started experimenting with it in low mode. The rocker switch is in the middle position for that. I set the knobs in the middle of the ranges and then played with it from there.
In high pulse the A/C frequency can mask the pulse but it is happening, you just have to play with the adjustments until you figure out where you like it. 
If your pedal is working correctly then try adding a little upslope and downslope. I was playing with it today and found it was a lot smoother comming on and getting off the pedal. Also if you use a high A/C freq setting because it feels better your arc will be wider and the changes in current won't be as dramatic as they are with a lower frequency and tighter arc.
				
			 
			
		 
			
				
			
			
				Steve
Miller 212
Everlast 250EX
Everlast PowerPlasma 60
Victor O/A 
Current Project: 21' Jet Sled Rat Boat.