    Default Binzel Type mig gun question

    I have a new I 200 mig with the Binzel type gun and the contact tip is recessed in the nozzle by more then 1/8 inch, 0.159 to be exact. I cannot figure out how to get the even (+ -) with the end of the nozzle.
    I guess I am missing the obvious but any help would be appreciated.
    Ray

  2. #2

    Default

    The tips is supposed to be recessed. This is not a design flaw or defect. Put a longer tip in and you will not be happy...trust me.

  3. #3

    Default

    A longer tip and you will lose the needed gas for a good weld, as well the burnback will probably mess up the contact tip.

    The tip is recessed, as Mark said, that is normal.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. #4

    Default

    Quote Originally Posted by Ram48 View Post
    I have a new I 200 mig with the Binzel type gun and the contact tip is recessed in the nozzle by more then 1/8 inch, 0.159 to be exact. I cannot figure out how to get the even (+ -) with the end of the nozzle.
    I guess I am missing the obvious but any help would be appreciated.
    Ray
    I have an AK25 gun on an Imig 205, I got a seperate cup and used the lathe to knock off a little over .100 thous. to get into corners and 90 degree fillets
    You need to up the gas a little and watch for burnback,,, on normal welds I change back to the original or just slide it a head slightly, seems to work for me. Everybody holds the gun different and moves at a different pace, what ever makes you happy is whats counts.

Similar Threads

  1. Tig torch switch type?
    By Skeeter in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 01-18-2017, 03:38 AM
  2. Type of shielding gas used.
    By dyethor in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 16
    Last Post: 05-01-2012, 04:18 PM
  3. Trifamet / Binzel Mig torch Question
    By SeanMurphy265 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 4
    Last Post: 01-24-2012, 10:25 PM
  4. Which Binzel torch comes with the IMIG205P?
    By dlcain in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 2
    Last Post: 05-24-2011, 04:13 PM
  5. torch type questions
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 03-31-2011, 07:14 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •