 Originally Posted by 
WAYNESWORLD
					 
				 
				You can remove the outer heavy sleeve from the torch and replace it with the flexible braided cover. It will increase the flexibility quite a bit especially in colder temperatures. 
   Wayne
			
		 
	 
 You could also replace the hoses with CK superflex and make a really big difference. The Everalst torch is not a bad torch. I think it's the jacket and cables that make it unwieldly. I can't wait for the spring thaw myself. I'm getting tired of all my coiled up cords and hoses not wanting to uncoil. LOL..
I use CK torches mostly but I also use the Everlast often enough that I'm not going to discount it's value.
				
			 
			
		 
			
				
			
			
				Steve