I have the PowerTig 225LX and have been playing this morning. I have learned some stuff but now have even more questions for you learned types. Some of this stuff may seem really stupid, but I'd rather ask than keep wondering.
First the machine settings: 30 amps, AC, 2T-w/torch switch, Pulse OFF,
1/16" 2% thoriated, no. 5 gas cup, 100% argon @ 6 LPH.
Type metal: .025 aluminum sheet (Lowes), 4043 1/16" rod.
Questions
I seem to be unable to change the amount of cathotic etching with the AC balance. On a nice consistent .25 inch wide bead the etching is about 2/3 as wide on both sides of the bead, with no apparent change no matter what the setting of the AC balance. Is this normal at lower amps?
When pulse is selected and you use an amperage setting of say 30 amps and the display flashes between 2 numbers, I understand that to indicate the high and the low amperage while pulsing. Why do these numbers wander?
If I set the amps to the lowest setting (23 amps on my machine) with pulse selected will there be any observable difference (will it pulse lower)?
Does the up slope and down slope function in 2T mode utilizing the torch switch? (Ie. ramp up to set amperage and then ramp down or is this only in 4T?)
On initial start I sometimes get a crackle and/or a sputter on the above listed aluminum. Is this caused by my technique or is it something I've not set up correctly? (not enough gas flow, dirty metal/poor quality metal, electrode gap, electrode stickout, torch angle, etc.)
How long should my Argon last? I've got a 160CF bottle that started with 2200lbs of pressure. after 2.5 hours of actual torch lit time @6 LPH I have about 1800lbs of pressure. Is this normal? My mig machine doesn't seem to go thru gas quite as quickly!? (I plan on bubble checking it later)
What is the air speed velocity of an unladen swallow? (african)
I'd appreciate any insight you folks might have.
Best Regards, Zoom