Share
Page 4 of 4 FirstFirst ... 234
Results 61 to 63 of 63

Thread: Cut50d

  1. #61

    Default

    Quote Originally Posted by kenwhite View Post
    Thanks Mike and the cutter has been working great! I will be cutting some 3/16" thick crusher corners for my TJ later next week so I will try and post a few before/after pictures.
    Good to hear Ken.

    Another Jeep guy. My son has a friend that has two monster Jeeps. They go out every weekend, in fact he's not here now. They also race them and do very well, but they break them as well. They race on a short mud drag strip, and those things fly. Just 2-3 seconds and the race is over (parts are broke, etc).

    What do you with yours? Off-road, crawling, is it a new project.

    Like to see the before and after myself. On the L135, you will need a bigger welder soon.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  2. #62

    Default

    I primarily do rock crawling or anything technical. My entire suspension will be removed and replaced with new links and brackets. Oh, and I know my baby MIG will be pushed to the limits, I should have purchased a 240 VAC unit...
    __________________________
    Everlast Power I-MIG 200
    Everlast PowerUltra 205P
    Everlast SM 200-N
    Thermal Dynamics Cutmaster 42

  3. #63

    Default

    Just wanted to bump this up and state that the Cut50D is still working flawlessly after the initial issue...

    __________________________
    Everlast Power I-MIG 200
    Everlast PowerUltra 205P
    Everlast SM 200-N
    Thermal Dynamics Cutmaster 42

Similar Threads

  1. My new CUT50D
    By Butchmullins1 in forum Introduce Yourself
    Replies: 1
    Last Post: 03-21-2009, 04:13 PM
  2. broken cut50D, no help
    By ace-driver in forum Customer Testimonials
    Replies: 4
    Last Post: 01-10-2009, 04:01 AM
  3. Just got the Cut50D going today
    By andrewhotrod in forum Introduce Yourself
    Replies: 2
    Last Post: 12-11-2008, 11:55 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •