    I have used my Power Ultra 205 several times since receiving it in mid June but encountered my first problem with it tonite. I was cutting some 1/8 thick square tubing with the plasma cutter and the machine began to make an audible arcing/hissing/snapping sound inside. The indicator LEDs went out but the fans continued to run. I shut it off for several minutes and tried it again...that same arcing/hissing/snapping sound. I looked through the finned grill work on the front of the machine and could see arcing within. I don't know what to do now...please help. :cry:
    BigMacWelds
    Everalst PowerMaster 226 Combo Unit (TIG/Arc/Plasma)
    Hobart Handler 210 (MIG)

    If it breaks, weld it; If it's not broken, you're not using it hard enough...

  2. Default Re: Power Ultra 205 Plasma Problems

    BigMacWelds,

    Nice talking to you and very sorry we could not run all the testing I would have liked. I sent an email also where we left off on debugging the unit. Ask for ext. 201 and they will take care of you from here.
    Mike R.
    http://www.everlastwelders.com
    http://www.everlastgenerators.com

  3. Default Re: Power Ultra 205 Plasma Problems

    everlast_support,

    Yes...it was good talking with you, too. Thanks for the quick reply (phone call). Although I'm disappointed that the unit isn't working right, I am happy about all the great support Everlast is providing. Mike R (Tech Support), Alex, Katya, and the rest...you are really going out of your way to makes things right. That means a lot to me. I look forward to getting this straightened out. Thanks again for all the help...
    BigMacWelds
    Everalst PowerMaster 226 Combo Unit (TIG/Arc/Plasma)
    Hobart Handler 210 (MIG)

    If it breaks, weld it; If it's not broken, you're not using it hard enough...

Similar Threads

  1. Power Ultra 205 Plasma amps not correct
    By Zaichuk in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 09-16-2017, 05:17 AM
  2. New Feature / Plasma Torch for Power Ultra 205
    By Titan winch in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 10
    Last Post: 06-03-2011, 08:05 PM
  3. Problems with Power Plasma 50
    By Mattox in forum Everlast Plasma Cutters (PAC)
    Replies: 0
    Last Post: 11-02-2010, 05:49 PM
  4. Everlast Power Ultra 205 plasma cut
    By worntorn in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 06-17-2010, 03:59 PM
  5. Power Ultra 205 Plasma Ceramic Tip with guide ridge?
    By ralphhood3 in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 05-20-2010, 09:49 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •