    arch zone and weld depot are the best two I have found so far. Any others out there worth taking a look at?
    sold my miller mig
    got a PT250EX
    saving up for a plasma cutter

  2. #2

    Default

    I have purchased gas cups and other welding minutia via EBay with pretty decent success. I must say I really like walking into the LWS and getting stuff though. I've established a pretty good relationship and can get stuff now and at reasonable prices.
    PowerTig 225LX
    PowerCool W300
    PowerPlasma 60S
    Miller 140 MIG

  3. #3

    Default

    I just ordered my Miller Elite Digital helmet and some Weld Craft tungsten and some filler rod from http://www.weldingsupply.com/
    The helmet ran me $287 rather then the $390 everyone else wants for it. They also had really good prices for the tungsten and filler rods. I purchased 2 pounds of 3 sizes of ER70S2 and 308L and 5 sizes of 4043 (22lbs total), the helmet, Tillman gloves, and 3 different sized tungsten all for less than $500.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  4. #4

    Default

    I work away from home weekdays and home on weekends so It can make a little home project stretch for weeks if I try to mail order everything I "might" need. It can be very hard (and frustrating) to predict what type materials may be needed for a given project.
    PowerTig 225LX
    PowerCool W300
    PowerPlasma 60S
    Miller 140 MIG

  5. #5

    Default

    WeldMart, and harbor freight are great, with different needs of course.

  6. #6

    Default

    Quote Originally Posted by performance View Post
    WeldMart, and harbor freight are great, with different needs of course.
    mark, i've always read/heard to stay away from harbor frieght consumables..are the tig consumables from them of decent quality? i'd hate to fight with crappy consumables when im trying to figure this thing out! lol
    300whp FWD 94 Celica
    PowerPro 205 with a hack behind the mask!

  7. #7
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Be careful about Harbor Freight welding consumables unless you are really desperate. Some there are jaw-droppingly overpriced, like 1.1lb spool of 4043 aluminum filler wire for $30.
    http://www.harborfreight.com/11-lb-0...ire-42935.html

    If you put together a large enough size order to defray the shipping costs, weldingsupply.com has really great prices on most welding consumables and accessories like filler rod. They also have a pretty nice selection compared to the other online vendors. They do not ship it out immedaitely IME, but took a few days to package it up. So be sure to plan ahead with them.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  8. #8

    Default

    http://store.cyberweld.com/
    Has free shipping on orders over $25.00
    Gerald

    Millermatic 251
    Spectrum 300 Plasma
    Everlast PowerTig 250EX
    Everlast PowerCool W300
    Harris / Victor OA
    Craftsman 13 Speed Drill Press
    ProTools Air/Hydraulic Bender
    48" Brake, 72" Brake, 52" Stomp Shear
    Mitler Bros. 36" High Throat Bead Roller
    Compressor, Notchers, Grinders, etc.

  9. Default

    Free shipping was the clincher. I have my first order with them. Thanks for the post. I buy locally when I can, but the prices are just so high sometimes. I'll pay 20% more to support a local guy on smaller items, but the 300% higher than online is making me pretty damn mad.
    I am out trying to 'find myself'. If I should wander back while I am gone, please tell me to sit quietly and wait for myself to return.

    LOTS of scuba and vintage scuba equipment [I'm Always willing to trade or buy the stuff you think is too old to use]
    Smithy XLT Mill/lathe [It was easier to learn than I thought, I'm no pro, but I can make a bearing hanger]
    Everlast PP256

  10. #10

    Default

    Quote Originally Posted by jakeru View Post
    If you put together a large enough size order to defray the shipping costs, weldingsupply.com has really great prices on most welding consumables and accessories like filler rod. They also have a pretty nice selection compared to the other online vendors. They do not ship it out immedaitely IME, but took a few days to package it up. So be sure to plan ahead with them.

    I had no issue with weldingsupply shipping my stuff. They shipped it the day after I made the order and it only took 1 day to get to me.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  11. #11

    Default

    Arc zone has good pricing on tungsten and filler metal and that is the only place online where I could find 2% lanthanated electrodes. And you also get a free bag a peanuts with every order.

  12. #12

    Default

    Quote Originally Posted by ryanfull View Post
    And you also get a free bag a peanuts with every order.
    Don't you mean M&M's?
    Gerald

    Millermatic 251
    Spectrum 300 Plasma
    Everlast PowerTig 250EX
    Everlast PowerCool W300
    Harris / Victor OA
    Craftsman 13 Speed Drill Press
    ProTools Air/Hydraulic Bender
    48" Brake, 72" Brake, 52" Stomp Shear
    Mitler Bros. 36" High Throat Bead Roller
    Compressor, Notchers, Grinders, etc.

  13. #13
    Join Date
    Mar 2011
    Location
    mission viejo CA
    Posts
    92

    Default

    stay away from toughweld.com unless you want your stuff a month or so later
    Lincoln precision tig 275
    Miller Syncrowave 350 Tig
    Miller 250 Mig
    old miller 200 Mig
    HF 151 Mig
    HF 100 FC
    Victor Journeyman Oxy/Ace set up
    Bunch of tools of the trade to much to list

  14. #14

    Default

    Not an expert yet. However, from what I have read arc-zone is one of the better online to deal with. I have ordered from them more than once. I have had no problems. I didnt get a free bag of peanuts though.
    Frank

    I have a 250 EX welder and several other machines and equipment to allow for small scale manufacturing and prototyping of inventions

    I am located in Oregon about 20 minutes west of Portland

  15. #15

    Default

    Ya I meant m&m's
    Hobart 140 mig
    Century 300 amp AC stick
    PP256
    Oxy-Accetylene torch
    Milwaukee 14" chop saw
    Evolution compound miter cold cut saw

  16. #16

    Default

    after looking around it looks like wed depot has the best prices that I can find
    sold my miller mig
    got a PT250EX
    saving up for a plasma cutter

  17. #17
    Join Date
    Apr 2011
    Location
    Sasktachewan, Canada
    Posts
    95

    Default

    Great list of possible suppliers, I will have to check out a few of them. Free shipping can be a real deal clincher.
    Attitude Determines Altitude

  18. #18
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default Cyberweld

    Just had a great experience with Cyberweld- based on this thread I placed an order on Friday. Shipping was free, and the new helmet was FedExed and arrived Saturday morning. Wow!
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  19. #19
    Join Date
    Oct 2010
    Location
    Queensland, Australia
    Posts
    23

    Default

    I’ve been very happy with www.WeldFabulous.com as they had good prices and decent rates for overseas shipping. Not all of the others will ship international. I got a great deal on my Speedglas helmet from them.

    Chris
    Brisbane Australia.

Similar Threads

  1. Best/favorite online source for filler?
    By Trip59 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 10
    Last Post: 10-26-2012, 08:27 PM
  2. I ran across a place that sells metal and other tools.
    By Brian Ski in forum General Welding Questions
    Replies: 28
    Last Post: 04-08-2012, 09:51 PM
  3. parts / cons for 200dx stock tourch?
    By cboggs in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 01-11-2012, 02:13 PM
  4. using a coiled mig gun in place of the arc stick welder
    By britstef in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 07-17-2010, 01:38 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •