Share
Results 1 to 19 of 19

Thread: I bought a 200DX welder a week ago....

  1. #1

    Default I bought a 200DX welder a week ago....

    I have done some steel, and steel is super easy compared to aluminum.

    Well I have been practicing everyday for about 20-30 minutes.

    Here is about 2 hours of practice. Just to say, when I first started, I couldn't even get a arc without blowing the tungsten off. LOL.

    Purple Fabricator 211i

  2. #2

    Default

    looking good
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  3. #3

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    looking good
    Thanks! Anything I am doing wrong?
    Purple Fabricator 211i

  4. #4

    Default

    not really just welds a little wider when coming to end but it look good , it get wider at end because your aluminum gets hotter while welding so need to back off on pedal a little when aluminum is heated up
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  5. #5

    Default

    Not to get off topic but yours is a 2012 model right? I've been told the control panel is different from last year’s model could you please post a picture of the controls … I’m planning on buying one and I’m curious as to how it appears … thanks in advance ... by the way your bead looks great ... no porosity nice and even … really looks awesome.
    Winky B.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  6. #6

    Default

    Quote Originally Posted by Winky View Post
    Not to get off topic but yours is a 2012 model right? I've been told the control panel is different from last year’s model could you please post a picture of the controls … I’m planning on buying one and I’m curious as to how it appears … thanks in advance ... by the way your bead looks great ... no porosity nice and even … really looks awesome.
    Winky B.
    Thanks. Mine isn't the 2012 machine, I think. But I will post a pic for you in a minute.
    Purple Fabricator 211i

  7. #7

    Default

    Purple Fabricator 211i

  8. #8

    Default

    Quote Originally Posted by 225 View Post
    Thanks. Mine isn't the 2012 machine, I think. But I will post a pic for you in a minute.
    Ah ... you must be right ... was told there was an up slope adj ... evidently not on yours. When in 2T or 4T is the preset up slope adequite for your needs? Pedal control is better anyway. Even if there is no upslope control I'm ganna buy the 200DX ... looks like a sweet machine.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  9. #9

    Default

    I put a slot machine arm on the side of my tig machine lol. I pull the handle and all the knobs spin and were they stop at' is what i weld at lol
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  10. #10

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    I put a slot machine arm on the side of my tig machine lol. I pull the handle and all the knobs spin and were they stop at' is what i weld at lol
    Does your machine ever spit out quarters? Let me know if it does and I'll put slot machine arms on all of my equipment ... LMAO
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  11. #11

    Default

    lol no just spits out penny's lol
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  12. Default

    Quote Originally Posted by Winky View Post
    Ah ... you must be right ... was told there was an up slope adj ... evidently not on yours. When in 2T or 4T is the preset up slope adequite for your needs? Pedal control is better anyway. Even if there is no upslope control I'm ganna buy the 200DX ... looks like a sweet machine.

    New one is only available in Canada at the moment. It will be later this year before it's available here, last I read.

    I can't remember exactly when though. I can't decide whether to go ahead and get a 200DX, wait for the new one or get something a little bigger now so I get more features and don't have to wait.

    Also, to the original poster: If I can make beads like that on aluminum after 2 hours, I will be ecstatic. Much previous welding experience?
    Last edited by ncsugrad2006; 05-11-2012 at 01:24 AM.

  13. #13

    Default

    Quote Originally Posted by ncsugrad2006 View Post
    New one is only available in Canada at the moment. It will be later this year before it's available here, last I read.

    I can't remember exactly when though. I can't decide whether to go ahead and get a 200DX, wait for the new one or get something a little bigger now so I get more features and don't have to wait.

    Also, to the original poster: If I can make beads like that on aluminum after 2 hours, I will be ecstatic. Much previous welding experience?
    Thanks ... I will be making an upgrade soon and I have had my heart set on the 200DX so I will probably go ahead and get that one ... I probably will be doing most of my welding with the pedal ... I'm curious as to what the preset up-slope setting is in the triggered mode.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  14. #14

    Default

    Quote Originally Posted by ncsugrad2006 View Post

    Also, to the original poster: If I can make beads like that on aluminum after 2 hours, I will be ecstatic. Much previous welding experience?
    I am 33. When I was 18, I was certified in pipe welding using stick. But now I am so horrible at stick welding, I won't show my work on here.

    I am familiar with welding. Haven't touched it in 10+ years. Never touched a TIG torch until last week.


    Thanks for the compliment.
    Purple Fabricator 211i

  15. #15

    Default

    I like stick welding but i stick weld everything thicker than 1/2 inch since i know it will be a deep weld
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  16. Default

    Quote Originally Posted by Winky View Post
    Thanks ... I will be making an upgrade soon and I have had my heart set on the 200DX so I will probably go ahead and get that one ... I probably will be doing most of my welding with the pedal ... I'm curious as to what the preset up-slope setting is in the triggered mode.
    I believe Jodi at weldingtipsandtricks.com has a video on that that shows it very well. It's basically exactly what it sounds like, where when you hit the trigger on the torch it slows ramps up the amperage over however long the machine is set for (assuming this one is adjustable, I can't remember for sure whether it is or isn't). That way you get the benefit of being able to ramp amperage up and the beginning and down at the end without using a foot pedal.

    Here's a page on it, but can't find the video

    http://www.weldingtipsandtricks.com/...ngs-part3.html

  17. #17

    Default

    Quote Originally Posted by ncsugrad2006 View Post
    I believe Jodi at weldingtipsandtricks.com has a video on that that shows it very well. It's basically exactly what it sounds like, where when you hit the trigger on the torch it slows ramps up the amperage over however long the machine is set for (assuming this one is adjustable, I can't remember for sure whether it is or isn't). That way you get the benefit of being able to ramp amperage up and the beginning and down at the end without using a foot pedal.

    Here's a page on it, but can't find the video

    http://www.weldingtipsandtricks.com/...ngs-part3.html
    Thanks ... I've seen the video ... Jodi is great ... love his web site. What I was wondering ... on the model of the 200DX that only has a down slope control ... is an internal preset so when you fire up the torch in 2t 4t the arc doesn't start up with it's full intensity ... this could creat issues with thin metal.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  18. Default

    Quote Originally Posted by Winky View Post
    Thanks ... I've seen the video ... Jodi is great ... love his web site. What I was wondering ... on the model of the 200DX that only has a down slope control ... is an internal preset so when you fire up the torch in 2t 4t the arc doesn't start up with it's full intensity ... this could creat issues with thin metal.
    I believe it does have a preset of some sort. I think I saw it on the webpage where you can buy that model, or maybe it's on the page that compares the different models.

  19. #19

    Default

    Quote Originally Posted by ncsugrad2006 View Post
    I believe it does have a preset of some sort. I think I saw it on the webpage where you can buy that model, or maybe it's on the page that compares the different models.
    Thanks ... I'll have another look.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

Similar Threads

  1. Just received Dual Voltage 200DX TIG Welder
    By MBfrontier in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 10-28-2013, 12:41 PM
  2. NEW 2013 Everlast PowerTIG 200DX AC/DC TIG DUAL VOLTAGE welder
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 28
    Last Post: 03-04-2013, 02:23 AM
  3. Think I might order my 200DX this week
    By Winky in forum Pre-sales, Sales and Shipping questions
    Replies: 34
    Last Post: 06-03-2012, 12:57 AM
  4. Powertig 200DX fairly new TIG welder
    By chevyracer56 in forum Introduce Yourself
    Replies: 40
    Last Post: 08-27-2011, 11:57 PM
  5. Just bought a welder? Read this!
    By performance in forum Welding articles from Professionals (knowledge database)
    Replies: 3
    Last Post: 04-04-2011, 08:40 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •